Gorffeniad cotio dur SGCH:
R (spangle arferol), Z (sbangle wedi'i leihau)
Dur SGCH Ansawdd wyneb coil / stribed / dalen:
A (Fel arwyneb gorchuddio), B (Arwyneb Gwell), C (Arwyneb Ansawdd Gorau)
Triniaeth arwyneb coil / stribed / dalen ddur SGCH:
C (Triniaeth cromad), NC (triniaeth nad yw'n Cromad), O (olew), X (dadlifo) NP (Triniaeth ffosffatio nad yw'n gromad), P(Phosphated), M (Heb ei drin)
Coil / stribed dur SGCH / màs cotio dalen:
Gorchudd Sinc Pur: Z06 (60g), Z08(80g), Z10(100g), Z12(120g), Z14(140g), Z18(180g), Z20(200g), Z22(220g), Z25(250g), Z27 (270g), Z35(350g), Z37(370g), Z45(450g), Z60(450g)
Aloi Sinc+Fe: F04(40g), F06(60g), F08(80g), F10(10g0), F12(120g), F18(180g)
Dur SGCH Coil / stribed / gorchudd dalen: Z (Sinc Pur), ZF (aloi Z + Fe)
JIS G 3302 SGCH dur maint addas: Trwch 0.11mm-1.0mm
Cyfansoddiad cemegol dur SGCH % :
| Gradd | C uchafswm | M max | P max | S max |
| SGCH | 0.18 | 1.20 | 0.08 | 0.05 |
SGCH dur dur Priodweddau mecanyddol
| Gradd | Cryfder Cynnyrch MPa | Cryfder tynnol MPa | Elongation % mun | |||||
| {{0}}.25- Llai na neu'n hafal i 0.40mm | {{0}}.40- Llai na neu'n hafal i 0.60mm | {{0}}.60- Llai na neu'n hafal i 1.0mm | 1.0- Llai na neu'n hafal i 1.6mm | 1.6- Llai na neu'n hafal i 2.5mm | Uwchben 2.5mm | |||
| SGCH | - | - | - | - | - | - | - | - |
Mae gan GNEE STEEL fwy na 2000 tunnell o ffynhonnell stoc dur SGCH bob mis. Gallwn gwrdd â'r rhan fwyaf o'n cwsmeriaid o ran maint a chais technegol. Yn seiliedig ar y ffynhonnell stoc hyn, ymledodd ein diwydiant mantais i broses ddur fel: torri (ar led a hyd), lluniadu, ail-bacio, ac ati.